Impact of repeated heat-pressing on the microstructure and flexural strength of lithium disilicate glass-ceramics
The mechanical properties of LDGC significantly degraded after repeated heat pressing. Therefore, it is not clinically advisable to repeatedly press the lithium disilicate ingot together with the leftover material.
Authors
- Fu Wang (ORCID: https://orcid.org/0000-0001-9222-0833)
- Qi Wang (ORCID: https://orcid.org/0000-0002-5287-6050)
- Zhenzhen Zhang (ORCID: https://orcid.org/0000-0002-2041-7757)
- Li Ding (ORCID: https://orcid.org/0000-0003-1517-2975)
- Jiale Li
Institutions
- Xi’an University of Posts and Telecommunications (CN)
- Air Force Medical University (CN)
Publication Details
- Journal
- BMC Oral Health
- Published
- 2024-09-28
- DOI
- https://doi.org/10.1186/s12903-024-04933-z
- Citations
- 4
- Primary Topic
- Advanced ceramic materials synthesis
- Type
- article
- Field-Weighted Citation Impact
- 0.93
Funders
- National Natural Science Foundation of China
- Natural Science Foundation of Shaanxi Province