Microwave Hybrid Sintering and Soldering of Cu-Cr-W Composite Material for Reactive Power Breakers
Over 60% of reported failures for reactive power compensation systems are given for damage to electrical circuit breaker contacts. This paper presents a study on the development of microwave technology for sintering of W-Cu-Cr alloys at 1012 °C for 65 min using 623.38 W microwave power, as well as microwave joining at 231 °C of the W-Cu-Cr composite material on body contact using 475 W microwave power for 55 s. The joined components were subjected to mechanical and electrical tests in accordance with ICE standards to validate the applied technology. Tests of connection-disconnection of the electrical contacts were carried out in accordance with the maximum number of disconnections allowed by the manufacturer (2 cycles/min): 25 s rest time and 5 s operating time under load. The components of the electrical contact after 111237 switches were analyzed under a microscope revealing a reduction of the damaged area by 27% compared with the original contact.
Authors
- Cristian Daniel Ghelsingher
- Andrej Dávid (ORCID: https://orcid.org/0000-0002-4820-6521)
- Sorin Vasile Savu (ORCID: https://orcid.org/0000-0002-0623-5244)
- Claudiu Nicolicescu (ORCID: https://orcid.org/0000-0001-9732-202X)
- Iulian Ştefan (ORCID: https://orcid.org/0000-0001-9661-897X)
- Ionel Dănuţ Savu (ORCID: https://orcid.org/0000-0002-0058-2405)
- Nicușor-Alin Sîrbu (ORCID: https://orcid.org/0000-0003-4229-0627)
- Ilie Dumitru (ORCID: https://orcid.org/0000-0002-1049-9680)
- Andrei-Angelo Midan
Institutions
- University of Žilina (SK)
- National Institute for Research and Development in Welding and Material Testing (RO)
- University of Craiova (RO)
Publication Details
- Journal
- Materials
- Published
- 2024-09-22
- DOI
- https://doi.org/10.3390/ma17184648
- Citations
- 2
- Primary Topic
- Electrical Contact Performance and Analysis
- Type
- article
- Field-Weighted Citation Impact
- 0.43