Brass corrosion – dezincification in hydrochloric acid
Abstract Brass is among the utility metals for daily life. We present an easy corrosion experiment for demonstration in high school or first-year undergraduate studies. Almost any kind of brass can be dezincified in 1 m hydrochloric acid. Copper as the noble component remains as salmon pink coating on the workpiece while zinc and lead, the latter being a frequent minor alloying component of brass, are dissolved. Lead can be detected as PbS ( in-situ generation of H 2 S from a splinter of FeS or as PbI 2 using KI). Zinc can be analyzed as Rinmann’s green or via a microchemical drop reaction with dithizone.
Authors
- Rainer Pöttgen (ORCID: https://orcid.org/0000-0003-0962-279X)
- Olaf Reckeweg (ORCID: https://orcid.org/0000-0003-1659-8644)
- Jasmin Schröer
- Thomas Fickenscher
Institutions
- University of Münster (DE)
- Hermann Staudinger Gymnasium (DE)
Publication Details
- Journal
- Zeitschrift für Naturforschung B
- Published
- 2024-09-17
- DOI
- https://doi.org/10.1515/znb-2024-0052
- Primary Topic
- Metallurgy and Material Science
- Type
- article
- Field-Weighted Citation Impact
- 0.00