Alloy scattering to optimize carrier and phonon transport properties in PbBi2S4 thermoelectric

Ternary PbBi 2 S 4 compound with crustal S-rich element and low lattice thermal conductivity is considered as a potential thermoelectric candidate. However, its inferior thermoelectric properties are rooted in the low electrical transport performance. Generally, enhancing electrical transport performance (power factor, PF) primarily entails optimizing the interdependent relationship between carrier mobility μ (linked to electrical conductivity σ ) and effective mass m ∗ (related to Seebeck coefficient S ). In this work, we introduce the strategy of alloy scattering to independently enhance S without weakening μ and simultaneously reduce thermal conductivity, leading to a synergetic optimization of electron and phonon in PbBi 2 S 4 thermoelectric. Heavy Sn alloying in PbBi 2 S 4 presents uniform and orderly distribution on Pb sites as unclosed by the atomic-scale crystal structure observation. These massive Sn atom serves as scattering centers and turns the electron scattering mechanism to be dominated by alloy scattering, thus resulting in a ∼33% increment of S in Pb 0.6 Sn 0.4 Bi 2 S 4 . Meanwhile, Sn alloying aggravates phonon scattering further lowering lattice thermal conductivity and reaching an extremely low value of 0.34 W⋅m −1 ·K −1 at 773 K. Finally, a maximum zT of 0.68 at 773 K is obtained in Pb 0.6 Sn 0.4 Bi 2 S 4 , which is ∼ 45% higher than the pristine matrix. This study proves that the strategy of alloy scattering is effective in improving overall electrical transport properties as well as reducing lattice thermal conductivity, which paves a new way to develop high-performance thermoelectric materials. • Heavy Sn alloying changes the scattering mechanism of the pristine PbBi 2 S 4 . • Demonstrate the feasibility of alloy scattering. • The highest zT value 0.68 is achieved for PbBi 2 S 4 -based material in Pb 0.6 Sn 0.4 Bi 2 S 4 .

Authors

Institutions

Publication Details

Journal
Journal of Materiomics
Published
2024-09-12
DOI
https://doi.org/10.1016/j.jmat.2024.100938
Citations
11
Primary Topic
Advanced Thermoelectric Materials and Devices
Type
article
Field-Weighted Citation Impact
1.29

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Alloy scattering to optimize carrier and phonon transport properties in PbBi2S4 thermoelectric

Liqing Xu, Wei Liu, Guilong Yan, Yu Xiao et al.
11 citations
Journal of Materiomics
Advanced Thermoelectric Materials and Devices
1.29
article

Alloy scattering to optimize carrier and phonon transport properties in PbBi2S4 thermoelectric

Liqing Xu, Wei Liu, Guilong Yan, Yu Xiao, Tao Hong, Wenke He, Xinxiu Cheng
article en
11 citations

Abstract

Ternary PbBi 2 S 4 compound with crustal S-rich element and low lattice thermal conductivity is considered as a potential thermoelectric candidate. However, its inferior thermoelectric properties are rooted in the low electrical transport performance. Generally, enhancing electrical transport performance (power factor, PF) primarily entails optimizing the interdependent relationship between carrier mobility μ (linked to electrical conductivity σ ) and effective mass m ∗ (related to Seebeck coefficient S ). In this work, we introduce the strategy of alloy scattering to independently enhance S without weakening μ and simultaneously reduce thermal conductivity, leading to a synergetic optimization of electron and phonon in PbBi 2 S 4 thermoelectric. Heavy Sn alloying in PbBi 2 S 4 presents uniform and orderly distribution on Pb sites as unclosed by the atomic-scale crystal structure observation. These massive Sn atom serves as scattering centers and turns the electron scattering mechanism to be dominated by alloy scattering, thus resulting in a ∼33% increment of S in Pb 0.6 Sn 0.4 Bi 2 S 4 . Meanwhile, Sn alloying aggravates phonon scattering further lowering lattice thermal conductivity and reaching an extremely low value of 0.34 W⋅m −1 ·K −1 at 773 K. Finally, a maximum zT of 0.68 at 773 K is obtained in Pb 0.6 Sn 0.4 Bi 2 S 4 , which is ∼ 45% higher than the pristine matrix. This study proves that the strategy of alloy scattering is effective in improving overall electrical transport properties as well as reducing lattice thermal conductivity, which paves a new way to develop high-performance thermoelectric materials. • Heavy Sn alloying changes the scattering mechanism of the pristine PbBi 2 S 4 . • Demonstrate the feasibility of alloy scattering. • The highest zT value 0.68 is achieved for PbBi 2 S 4 -based material in Pb 0.6 Sn 0.4 Bi 2 S 4 .

Journal of MateriomicsVol. 11(4)
University of Electronic Science and Technology of China (CN), Southwest Petroleum University (CN), Beihang University (CN), Xi'an Jiaotong University (CN)
National Natural Science Foundation of China
Openalex Percentile: Top 16%
Advanced Thermoelectric Materials and Devices
1.29
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.