MECHANICAL BEHAVIOUR OF ISTLE FIBRE COMPOSITE REINFORCED WITH EPOXY AND E-GLASS AT DIFFERENT FIBRE ORIENTATIONS

This paper was aimed to study the mechanical properties of Istle fibre composites. The process of fabrication was done by hand layup technique at three different fibre orientations i.e., unidirectional, bidirectional and 45 degrees inclined, and also its effect on tensile and flexural property that was studied in the Instron Testing Machine. The fibre volume ratio was kept uniform for the entire specimen as 50:50. The treatment of istle fibre was done with sodium hydroxide to increase the fibre matrix bonding. The effect of E-glass reinforcement has also been studied in both bending tests and flexural tests. The maximum tensile and bending modulus recorded were from unidirectional fibre specimen.

Authors

Institutions

Publication Details

Journal
Journal of Chemical Technology and Metallurgy
Published
2024-09-09
DOI
https://doi.org/10.59957/jctm.v59.i5.2024.10
Primary Topic
Structural Analysis of Composite Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

MECHANICAL BEHAVIOUR OF ISTLE FIBRE COMPOSITE REINFORCED WITH EPOXY AND E-GLASS AT DIFFERENT FIBRE ORIENTATIONS

D. Rama Prabha, Narendiranath Babu T, Yash Kalonia, Aditya Shinde et al.
Journal of Chemical Technology and Metallurgy
Structural Analysis of Composite Materials
article

MECHANICAL BEHAVIOUR OF ISTLE FIBRE COMPOSITE REINFORCED WITH EPOXY AND E-GLASS AT DIFFERENT FIBRE ORIENTATIONS

D. Rama Prabha, Narendiranath Babu T, Yash Kalonia, Aditya Shinde, Rohit Joshi
article en

Abstract

This paper was aimed to study the mechanical properties of Istle fibre composites. The process of fabrication was done by hand layup technique at three different fibre orientations i.e., unidirectional, bidirectional and 45 degrees inclined, and also its effect on tensile and flexural property that was studied in the Instron Testing Machine. The fibre volume ratio was kept uniform for the entire specimen as 50:50. The treatment of istle fibre was done with sodium hydroxide to increase the fibre matrix bonding. The effect of E-glass reinforcement has also been studied in both bending tests and flexural tests. The maximum tensile and bending modulus recorded were from unidirectional fibre specimen.

Journal of Chemical Technology and MetallurgyVol. 59(5)
Vellore Institute of Technology University (IN)
VIT University
Openalex Percentile: Top 85%
Structural Analysis of Composite Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.