Calibration of binding energy and clarification of interfacial band bending for the Al2O3/diamond heterojunction

Due to the presence of an intrinsic C 1s peak in diamond, it is impossible to calibrate its binding energies using the adventitious C 1s peak (284.8 eV) during x-ray photoelectron spectroscopy measurement. The absence of accurate binding energy measurement makes it challenging to determine the interfacial band bending for the oxide/diamond heterojunction. To overcome this issue, a net-patterned gold (Au) mask is applied to the boron-doped diamond (B-diamond) to suppress the charge-up effect and calibrate the binding energy using the standard Au 4f peak (83.96 eV). The B-diamond epitaxial layer shows downward band bending toward the surface with a valence band maximum of 0.85 eV. Upon the formation of Al2O3 using an ozone precursor through the atomic layer deposition technique, the B-diamond continues to exhibit downward band bending toward the Al2O3/B-diamond interface. However, the bending energy has reduced, potentially attributed to the modification of the oxygen vacancies on the B-diamond surface by the ozone precursor during the Al2O3 deposition.

Authors

Institutions

Publication Details

Journal
Applied Physics Letters
Published
2024-09-02
DOI
https://doi.org/10.1063/5.0230817
Citations
1
Primary Topic
Diamond and Carbon-based Materials Research
Type
article
Field-Weighted Citation Impact
0.12

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Calibration of binding energy and clarification of interfacial band bending for the Al2O3/diamond heterojunction

Bo Da, Jiangwei Liu, Tokuyuki Teraji, Yasuo Koide
1 citations
Applied Physics Letters
Diamond and Carbon-based Materials Research
0.12
article

Calibration of binding energy and clarification of interfacial band bending for the Al2O3/diamond heterojunction

Bo Da, Jiangwei Liu, Tokuyuki Teraji, Yasuo Koide
article en
1 citations

Abstract

Due to the presence of an intrinsic C 1s peak in diamond, it is impossible to calibrate its binding energies using the adventitious C 1s peak (284.8 eV) during x-ray photoelectron spectroscopy measurement. The absence of accurate binding energy measurement makes it challenging to determine the interfacial band bending for the oxide/diamond heterojunction. To overcome this issue, a net-patterned gold (Au) mask is applied to the boron-doped diamond (B-diamond) to suppress the charge-up effect and calibrate the binding energy using the standard Au 4f peak (83.96 eV). The B-diamond epitaxial layer shows downward band bending toward the surface with a valence band maximum of 0.85 eV. Upon the formation of Al2O3 using an ozone precursor through the atomic layer deposition technique, the B-diamond continues to exhibit downward band bending toward the Al2O3/B-diamond interface. However, the bending energy has reduced, potentially attributed to the modification of the oxygen vacancies on the B-diamond surface by the ozone precursor during the Al2O3 deposition.

Applied Physics LettersVol. 125(10)
National Institute for Materials Science (JP)
Japan Society for the Promotion of Science London, Ministry of Education, Culture, Sports, Science and Technology, Japan Science and Technology Agency, Core Research for Evolutional Science and Technology
Affordable and clean energy
Openalex Percentile: Top 60%
Diamond and Carbon-based Materials Research
0.12
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.