Replacement of conventional aggregates and fillers with steel slag and palm kernel shell ash in dense-graded asphalt mixtures

Large quantities of steel slag and palm kernel shell ash (PKSA) – waste products from steel production and palm oil milling, respectively – are generated annually in several countries, and their disposal is challenging. Meanwhile, the over-reliance on conventional rock aggregates for asphalt mixture production poses increasing sustainability challenges. This study investigated the potential of entirely replacing granite aggregates with steel slag and PKSA in a dense-graded asphalt mixture. Two sets of asphalt mixtures were prepared; the control mixture contained crushed granite aggregate and hydrated lime, while the other set incorporated steel slag as coarse aggregate and PKSA as fine aggregate and filler. Both mixture types utilized AC-30 viscosity-graded asphalt binder. The properties of the waste materials met the quality standards required for aggregates in asphalt mixture production. Both mixture types were designed according to the Marshall design procedure and were evaluated for durability (Cantabro abrasion loss), fatigue cracking Resistance, rutting Resistance, and moisture damage susceptibility. The Cantabro abrasion loss test indicated that the waste-based mixture was 3% less durable than the control. However, the cracking Resistance of the waste-based mixture was approximately twice that of the control. Even though the rapid rutting test indicated that the control mixture was slightly superior in rutting Resistance, the Marshall quotient suggested otherwise. Both mixture types exhibited similar moisture damage resistance. Overall, the steel slag and PKSA samples have shown high potential to replace virgin granite aggregates and lime in asphalt mixtures fully and are, thus, recommended for field performance evaluation and possible adoption.

Authors

Institutions

Publication Details

Journal
Journal of Sustainable Construction Materials and Technologies
Published
2024-08-20
DOI
https://doi.org/10.47481/jscmt.1536080
Citations
1
Primary Topic
Asphalt Pavement Performance Evaluation
Type
article
Field-Weighted Citation Impact
0.26

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Replacement of conventional aggregates and fillers with steel slag and palm kernel shell ash in dense-graded asphalt mixtures

Kenneth A. Tutu, Collins Abrefa Nketiah, David A. Azong-bil, Ebenezer D. A. Barnor
1 citations
Journal of Sustainable Construction Materials and Technologies
Asphalt Pavement Performance Evaluation
0.26
article

Replacement of conventional aggregates and fillers with steel slag and palm kernel shell ash in dense-graded asphalt mixtures

Kenneth A. Tutu, Collins Abrefa Nketiah, David A. Azong-bil, Ebenezer D. A. Barnor
article en
1 citations

Abstract

Large quantities of steel slag and palm kernel shell ash (PKSA) – waste products from steel production and palm oil milling, respectively – are generated annually in several countries, and their disposal is challenging. Meanwhile, the over-reliance on conventional rock aggregates for asphalt mixture production poses increasing sustainability challenges. This study investigated the potential of entirely replacing granite aggregates with steel slag and PKSA in a dense-graded asphalt mixture. Two sets of asphalt mixtures were prepared; the control mixture contained crushed granite aggregate and hydrated lime, while the other set incorporated steel slag as coarse aggregate and PKSA as fine aggregate and filler. Both mixture types utilized AC-30 viscosity-graded asphalt binder. The properties of the waste materials met the quality standards required for aggregates in asphalt mixture production. Both mixture types were designed according to the Marshall design procedure and were evaluated for durability (Cantabro abrasion loss), fatigue cracking Resistance, rutting Resistance, and moisture damage susceptibility. The Cantabro abrasion loss test indicated that the waste-based mixture was 3% less durable than the control. However, the cracking Resistance of the waste-based mixture was approximately twice that of the control. Even though the rapid rutting test indicated that the control mixture was slightly superior in rutting Resistance, the Marshall quotient suggested otherwise. Both mixture types exhibited similar moisture damage resistance. Overall, the steel slag and PKSA samples have shown high potential to replace virgin granite aggregates and lime in asphalt mixtures fully and are, thus, recommended for field performance evaluation and possible adoption.

Journal of Sustainable Construction Materials and TechnologiesVol. 9(3)
Kwame Nkrumah University of Science and Technology (GH), Kwame Nkrumah University (ZM)
Kwame Nkrumah University of Science and Technology
Responsible consumption and production
Openalex Percentile: Top 45%
Asphalt Pavement Performance Evaluation
0.26
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.