Advanced smectite alteration and the role of accessory reactants at 180 °C: New experimental constraints on the stability of bentonite

Bentonite clay is commonly accepted as an appropriate material for backfilling the space between the radioactive canisters and the host rock of planned underground repository sites for waste disposal. Despite its favourable properties as a hydrodynamic seal, its long-term stability remains a concern. This experimental study of a Bavarian bentonite investigated advanced montmorillonite (smectite) illitisation at 180 °C in the presence of K-oxalate and/or the accessory minerals of pyrite and calcite. The formation of mixed-layered illite-smectite was quantified by X-ray diffraction Rietveld refinement and the crystal chemistry was determined by transmission electron microscopy. The results showed neocrystallisation of a celadonitic illite-smectite (up to 63% illite-layers) after treatment with KCl or K-oxalate with increased Al 3+ in the tetrahedral sheets, reduced amounts in the octahedral locations and increased fixation of non-exchangeable K + ions in response to the increased layer charges. K-oxalate complexation of Al 3+ and enhanced dissolution of the smectite resulted in the formation of a possible intermediate amorphous phase and illite-smectite crystallites with additional vacant sites explaining the lower number of octahedral ions (<2 per formula unit). Adding 10% pyrite, 10% calcite, or 5% of each, did influence the degree of alteration to a recognisable degree in the presence of KCl, but the effects on the rate of illitisation were minimal when reacted with K-oxalate, which further increased illitisation by up to 6.4 times. Although batch reactor experiments do have limitations compared to complex repository conditions, our results do indicate that claystone host rocks low in organic matter should be favoured over organic-rich lithologies that are likely to contain oxalate ligands or similar catalysing compounds. • Experimental implications for the long-term stability of bentonite backfills. • Impact of organic ligands in catalyzing smectite-illitisation reactions. • Influence of accessory calcite and pyrite on montmorillonite stability.

Authors

Institutions

Publication Details

Journal
Applied Clay Science
Published
2024-09-01
DOI
https://doi.org/10.1016/j.clay.2024.107540
Citations
3
Primary Topic
Soil and Unsaturated Flow
Type
article
Field-Weighted Citation Impact
0.78

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Advanced smectite alteration and the role of accessory reactants at 180 °C: New experimental constraints on the stability of bentonite

Ritwick Sudheer Kumar, Laurence N. Warr, Balu R. Thombare, Georg Grathoff
3 citations
Applied Clay Science
Soil and Unsaturated Flow
0.78
article

Advanced smectite alteration and the role of accessory reactants at 180 °C: New experimental constraints on the stability of bentonite

Ritwick Sudheer Kumar, Laurence N. Warr, Balu R. Thombare, Georg Grathoff
article en
3 citations

Abstract

Bentonite clay is commonly accepted as an appropriate material for backfilling the space between the radioactive canisters and the host rock of planned underground repository sites for waste disposal. Despite its favourable properties as a hydrodynamic seal, its long-term stability remains a concern. This experimental study of a Bavarian bentonite investigated advanced montmorillonite (smectite) illitisation at 180 °C in the presence of K-oxalate and/or the accessory minerals of pyrite and calcite. The formation of mixed-layered illite-smectite was quantified by X-ray diffraction Rietveld refinement and the crystal chemistry was determined by transmission electron microscopy. The results showed neocrystallisation of a celadonitic illite-smectite (up to 63% illite-layers) after treatment with KCl or K-oxalate with increased Al 3+ in the tetrahedral sheets, reduced amounts in the octahedral locations and increased fixation of non-exchangeable K + ions in response to the increased layer charges. K-oxalate complexation of Al 3+ and enhanced dissolution of the smectite resulted in the formation of a possible intermediate amorphous phase and illite-smectite crystallites with additional vacant sites explaining the lower number of octahedral ions (<2 per formula unit). Adding 10% pyrite, 10% calcite, or 5% of each, did influence the degree of alteration to a recognisable degree in the presence of KCl, but the effects on the rate of illitisation were minimal when reacted with K-oxalate, which further increased illitisation by up to 6.4 times. Although batch reactor experiments do have limitations compared to complex repository conditions, our results do indicate that claystone host rocks low in organic matter should be favoured over organic-rich lithologies that are likely to contain oxalate ligands or similar catalysing compounds. • Experimental implications for the long-term stability of bentonite backfills. • Impact of organic ligands in catalyzing smectite-illitisation reactions. • Influence of accessory calcite and pyrite on montmorillonite stability.

Applied Clay ScienceVol. 260
Universität Greifswald (DE)
Deutsche Forschungsgemeinschaft, Bundesministerium für Wirtschaft und Technologie, Bundesministerium für Wirtschaft und Energie
Openalex Percentile: Top 30%
Soil and Unsaturated Flow
0.78
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.