Thermal decomposition kinetics and storage life prediction of nitramine propellants with different energetic plasticizers based on model-fitting method

The research on the thermal decomposition of propellant is critical to determining its safe storage life. The thermogravimetry (TG) testing of nitramine propellants plasticized by nitroglycerin (NG), glycidyl azide polymer (GAP), 2,2-dinitropropanol hexanoate (DNPH), and N-butyl-2-nitratoethylnitramine (BuNENA) was performed under non-isothermal circumstances. The thermal decomposition mechanism of propellant was then analyzed using the model-fitting method, and the storage life was predicted based on the mechanism. The results show that when heated to the same mass loss, the temperature of GAP-NC-RDX, BuNENA-NC-RDX, and DNPH-NC-RDX is higher than that of NG-NC-RDX. GAP-NC-RDX, BuNENA-NC-RDX, and DNPH-NC-RDX propellants have superior thermal stability to that of NG-NC-RDX. The kinetic mechanism functions and equations of the propellants were calculated, and multi-step reaction models of the thermal decomposition were built. The major thermal decomposition mechanism of nitramine propellants was discovered to be composite autocatalytic decomposition (Kamal-Sourour equation), which means that the reaction of reactants and the reaction catalyzed by products occur in tandem. The decomposition depth of propellants increases as the temperature rises during the same storage time. The storage lifetimes of GAP-NC-RDX, BuNENA-NC-RDX, DNPH-NC-RDX, and NG-NC-RDX propellants at 288 K are 28.71 years, 24.49 years, 18.34 years, and 16.33 years, respectively. The inclusion of GAP, DNPH, and BuNENA in the formulation improves the storage life of propellant more than NG. This study offers an attractive strategy for analyzing the decomposition mechanism of propellant with a multi-step decomposition reaction and forecasting its storage life.

Authors

Institutions

Publication Details

Journal
Case Studies in Thermal Engineering
Published
2024-08-23
DOI
https://doi.org/10.1016/j.csite.2024.105014
Citations
6
Primary Topic
Energetic Materials and Combustion
Type
article
Field-Weighted Citation Impact
1.62

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Thermal decomposition kinetics and storage life prediction of nitramine propellants with different energetic plasticizers based on model-fitting method

Xin Liao, Xiaoan Wei, Feiyun Chen, You Fu et al.
6 citations
Case Studies in Thermal Engineering
Energetic Materials and Combustion
1.62
article

Thermal decomposition kinetics and storage life prediction of nitramine propellants with different energetic plasticizers based on model-fitting method

Xin Liao, Xiaoan Wei, Feiyun Chen, You Fu, Bin Xu, Zhitao Liu, Yiqiang Long
article en
6 citations

Abstract

The research on the thermal decomposition of propellant is critical to determining its safe storage life. The thermogravimetry (TG) testing of nitramine propellants plasticized by nitroglycerin (NG), glycidyl azide polymer (GAP), 2,2-dinitropropanol hexanoate (DNPH), and N-butyl-2-nitratoethylnitramine (BuNENA) was performed under non-isothermal circumstances. The thermal decomposition mechanism of propellant was then analyzed using the model-fitting method, and the storage life was predicted based on the mechanism. The results show that when heated to the same mass loss, the temperature of GAP-NC-RDX, BuNENA-NC-RDX, and DNPH-NC-RDX is higher than that of NG-NC-RDX. GAP-NC-RDX, BuNENA-NC-RDX, and DNPH-NC-RDX propellants have superior thermal stability to that of NG-NC-RDX. The kinetic mechanism functions and equations of the propellants were calculated, and multi-step reaction models of the thermal decomposition were built. The major thermal decomposition mechanism of nitramine propellants was discovered to be composite autocatalytic decomposition (Kamal-Sourour equation), which means that the reaction of reactants and the reaction catalyzed by products occur in tandem. The decomposition depth of propellants increases as the temperature rises during the same storage time. The storage lifetimes of GAP-NC-RDX, BuNENA-NC-RDX, DNPH-NC-RDX, and NG-NC-RDX propellants at 288 K are 28.71 years, 24.49 years, 18.34 years, and 16.33 years, respectively. The inclusion of GAP, DNPH, and BuNENA in the formulation improves the storage life of propellant more than NG. This study offers an attractive strategy for analyzing the decomposition mechanism of propellant with a multi-step decomposition reaction and forecasting its storage life.

Case Studies in Thermal EngineeringVol. 61
Nanjing University of Science and Technology (CN), Luye Pharma (China) (CN)
China Postdoctoral Science Foundation
Responsible consumption and production
Openalex Percentile: Top 19%
Energetic Materials and Combustion
1.62
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.