Complex impedance studies of the precipitation-hardened lithium sodium niobate ferroelectrics
Precipitation hardening has been demonstrated as a good practice to suppress domain wall mobility and reduce losses in piezoceramics, especially when subjected to high-power drive. The hardening effect is generally determined by the morphology of precipitates introduced during the high-temperature aging treatment. In the present work, impedance spectroscopy is performed on the as-quenched and aged (Li, Na)NbO3 (LNN) solid solution to clarify the influence of aging treatment on the conductivity and electrical heterogeneity of LNN samples. The as-quenched LNN sample shows a lower resistivity due to higher oxygen vacancy concentration, which can be largely eliminated by reoxidation during the aging process. Moreover, the LiNbO3 (LN) precipitate-caused electrical heterogeneity is clarified by analyses of the impedance spectra fitted by an equivalent circuit and the activation energy calculated from relaxation peaks. The revealed impedance changes provide a foundation for future optimization strategies of precipitation-hardened piezoelectric ceramics.
Authors
- Changhao Zhao (ORCID: https://orcid.org/0000-0003-3739-8406)
- Xin Gao (ORCID: https://orcid.org/0000-0003-1308-3063)
- Mankang Zhu
- Mupeng Zheng (ORCID: https://orcid.org/0000-0001-7547-5025)
- Yudong Hou (ORCID: https://orcid.org/0000-0002-0981-3572)
- Jianing Shao
- Shuai An
Institutions
- Beijing University of Technology (CN)
- Xi'an Jiaotong University (CN)
Publication Details
- Journal
- Applied Physics Letters
- Published
- 2024-08-19
- DOI
- https://doi.org/10.1063/5.0225638
- Citations
- 3
- Primary Topic
- Ferroelectric and Piezoelectric Materials
- Type
- article
- Field-Weighted Citation Impact
- 0.35
Funders
- National Natural Science Foundation of China
- Natural Science Foundation of Beijing Municipality