Thermal cycling damage of silica refractories for high-temperature thermal energy storage (HT-TES) – Can it be healed?

Silica refractories are promising materials for high-temperature thermal energy storage (HT-TES), because they exhibit excellent thermal cycling properties, unless cooled below a critical temperature (usually assumed to be 600 °C). When cooling down to room temperature severe damage can occur, which can be conveniently monitored via the impulse excitation technique (IET). This damage is most severe when the cycling maximum temperature is low. The question is whether this damage can be healed again. In this short contribution we show that severe damage in silica refractories, caused by heating from room temperature to 300 °C and back again to room temperature, can indeed be healed by thermal cycling to 1300 °C. The healed material is actually better than the pristine material.

Authors

Institutions

Publication Details

Journal
Open Ceramics
Published
2024-08-13
DOI
https://doi.org/10.1016/j.oceram.2024.100658
Citations
5
Primary Topic
Recycling and utilization of industrial and municipal waste in materials production
Type
article
Field-Weighted Citation Impact
1.33

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Thermal cycling damage of silica refractories for high-temperature thermal energy storage (HT-TES) – Can it be healed?

Eva Gregorová, Willi Pabst, Lucie Kotrbová
5 citations
Open Ceramics
Recycling and utilization of industrial and municipal waste in materials production
1.33
article

Thermal cycling damage of silica refractories for high-temperature thermal energy storage (HT-TES) – Can it be healed?

Eva Gregorová, Willi Pabst, Lucie Kotrbová
article en
5 citations

Abstract

Silica refractories are promising materials for high-temperature thermal energy storage (HT-TES), because they exhibit excellent thermal cycling properties, unless cooled below a critical temperature (usually assumed to be 600 °C). When cooling down to room temperature severe damage can occur, which can be conveniently monitored via the impulse excitation technique (IET). This damage is most severe when the cycling maximum temperature is low. The question is whether this damage can be healed again. In this short contribution we show that severe damage in silica refractories, caused by heating from room temperature to 300 °C and back again to room temperature, can indeed be healed by thermal cycling to 1300 °C. The healed material is actually better than the pristine material.

Open CeramicsVol. 19
University of Chemistry and Technology, Prague (CZ)
European Commission, Ministerstvo Školství, Mládeže a Tělovýchovy
Affordable and clean energy
Openalex Percentile: Top 21%
Recycling and utilization of industrial and municipal waste in materials production
1.33
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Thermal cycling damage of silica refractories for high-temperature thermal energy storage (HT-TES) – Can it be healed? — Eva Gregorová, Willi Pabst, et al. · Open Ceramics (2024) | TGRS Research Map | TGRS