Utilization of polyacrylamide-thickening agent and aluminum sulfate liquid accelerator for improving early strength of Portland cement

There is a problem that accelerator make the early compressive strength of mortar develop slowly. This study to utilize thickening agent and developed accelerator to improve the early compressive strength. The research findings demonstrated that with the addition of accelerator, a large amount of hydration products is formed in the paste. The dosage of PAH was 2%, the strength of the mortar reached 13.96 MPa at 1 d. The primary cause is that the PAH formed a granule-particle bridge structure, which made the structure of hydration products denser, thus improving the early compressive strength. It provides the value for the application of accelerator and thickener in the shotcrete field.

Authors

Institutions

Publication Details

Journal
Materials Science and Technology
Published
2024-08-09
DOI
https://doi.org/10.1177/02670836241273472
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
article

Utilization of polyacrylamide-thickening agent and aluminum sulfate liquid accelerator for improving early strength of Portland cement

Zhihong Wu, Chunmei Li, LI Zhi-shun, Huafeng Zhou et al.
Materials Science and Technology
Concrete and Cement Materials Research
article

Utilization of polyacrylamide-thickening agent and aluminum sulfate liquid accelerator for improving early strength of Portland cement

Zhihong Wu, Chunmei Li, LI Zhi-shun, Huafeng Zhou, Wang Huang, Jiawei Wang, Wan Zhang, Yuexin Pan
article en

Abstract

There is a problem that accelerator make the early compressive strength of mortar develop slowly. This study to utilize thickening agent and developed accelerator to improve the early compressive strength. The research findings demonstrated that with the addition of accelerator, a large amount of hydration products is formed in the paste. The dosage of PAH was 2%, the strength of the mortar reached 13.96 MPa at 1 d. The primary cause is that the PAH formed a granule-particle bridge structure, which made the structure of hydration products denser, thus improving the early compressive strength. It provides the value for the application of accelerator and thickener in the shotcrete field.

Materials Science and TechnologyVol. 41(13)
Xi'an University of Architecture and Technology (CN), Ningxia Water Conservancy (CN), Institute of New Materials (CN)
National Natural Science Foundation of China
Openalex Percentile: Top 86%
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.